Standard: GOST 3282 – 74
Steel wire’s without heat - treatment rupture limit varies between 490 and 1,370 N/mm² subject to its diameter and steel grade.
Diameter, mm | Packing, kg | Output, m/kg | Type | Quantity, kg | Request |
---|---|---|---|---|---|
3,0 | on demand | ~18 | galvanized | Add | |
4,0 | on demand | ~10 | galvanized | Add | |
6,0 | on demand | ~4,5 | galvanized | Add | |
3,0 | on demand | ~18 | bright | Add | |
4,0 | on demand | ~10 | bright | Add | |
5,0 | on demand | ~6,5 | bright | Add | |
6,0 | on demand | ~4,5 | bright | Add |