Annealed bright Annealed wire’s rupture limit is 290 - 490 N/mm², elongation – at least 15-20% The wire is suitable for use in construction, household, industry, compressed was...
Annealed galvanised Annealed wire’s rupture limit is 340-540 N/mm², elongation – at least 12-18%. The wire is suitable for use in construction, household, industry. The wire is sof...
Spring Spring wire’s rupture limit varies between 1,230 and 2,740 N/mm² subject to its diameter. The spring wire is used in the furniture industry, production of house...
Without heat-treatment (solid) Standard: GOST 3282 – 74 Steel wire’s without heat - treatment rupture limit varies between 490 and 1,370 N/mm² subject to its diameter and steel grade.
Welding Raw steel wire’s rupture limit varies between 490 and 1,370 N/mm² subject to its diameter and steel grade.
Barbed Standard: GOST 285-69 Monobasic corrugated wire. Base wire thickness is 2,8 mm, barb wire thickness is - 2,0 mm. The zinc surface density should be not less tha...
Staples Standard: TU 14-4-1598-90E Staples are intended for wire and mesh fastening to wooden structures.
Double-loop bale tie Quicklink bale ties with double loop are used for binding bales. Wire coated with zinc. These bale ties were developed for binding highly expanding materials. ...